CHINESE JOURNAL OF ENERGETIC MATERIALS
+高级检索
低温下叠氮聚醚推进剂冲击损伤特性与动态力学性能
作者:
作者单位:

(1. 南京理工大学化工学院, 江苏 南京 210094; 2. 上海航天化工应用研究所, 浙江 湖州 313000)

作者简介:

郑启龙(1989-),男,博士,主要从事低燃温火药相关研究。e-mail: zhenglong2577@163.com 通信联系人: 肖乐勤(1972-),女,副研究员,主要从事含能材料相关研究。e-mail: leqinxiao@163.com

通讯作者:

肖乐勤(1972-),女,副研究员,主要从事含能材料相关研究。e-mail: leqinxiao@163.com

基金项目:

国家973重点基础研究规划项目资助(613275)


Impact Damage and Dynamic Mechanical Behaviors of Azido Polyether Propellant at Low Temperature
Author:
Affiliation:

(1. School of Chemical Engineering,Nanjing University of Science and Technology, Nanjing 210094, China; 2. Shanghai Aerospace Institute of Applied Chemical Engineering, Huzhou 313000, China)

Fund Project:

The National Basic Research Program of China (973 Program)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
    摘要:

    利用仪器化落锤冲击试验机在-40 ℃下对叠氮聚醚推进剂进行了冲击加载模拟实验, 通过X射线微层析成像技术(X-μCT)表征了推进剂的冲击损伤特性, 并采用动态力学分析研究了叠氮聚醚推进剂在不同加载频率下的动态力学性能。结果表明, 叠氮聚醚推进剂动态力学参数表现出显著的加载频率依赖性, 当加载频率由1 Hz增大至20 Hz时, 其玻璃化转变温度由-38.1 ℃升高至-23.1 ℃; 相应测试条件下, 推进剂试样在冲击加载能量不低于2 J时发生断裂, 未冲断推进剂无宏观裂纹产生, 但其内高氯酸铵(AP)颗粒已部分破碎; 被冲断试样冲击曲线中包含不稳定裂纹扩展过程, 表明叠氮聚醚推进剂在低温下具有一定的脆性材料特征, 推测其损伤模式为含缺陷的AP颗粒首先发生穿晶断裂, 初始微裂纹扩展于基体中并相互贯通扩大, 最终导致试样断裂。

    Abstract:

    The impact load was applied to azido polyether propellant by the instrumented drop hammer device at -40 ℃. The impact damage of the sample was characterized by X-ray micro-tomography (X-μCT), and the dynamic mechanical properties of the propellant sample were studied by dynamic mechanical analyzer at different loading frequencies. Results show that the dynamic mechanical properties of azido polyether propellant exhibit obviously loading frequency-dependent and the glass transition temperature increases from -38.1 ℃ to -23.1 ℃ when the loading frequency varies from 1 Hz to 20 Hz. The propellant samples have no macroscopic crack with the impact energy below 2 J, but part of the perchlorate amine(AP) particles inside have been broken; and the propellant samples break with the impact energy increasing. The test curves of broken samples contain unstable crack growth which indicates the partial brittle material character of azido polyether propellant. The whole process of the fracture of azido polyether propellant is that the initial micro cracks was formed in the AP particles with defects, extend to large macroscopic cracks in the basal body, and then the propellant samples broke.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

郑启龙,刘海涛,胡义文,等.低温下叠氮聚醚推进剂冲击损伤特性与动态力学性能[J].含能材料, 2017, 25(5):354-359. DOI:10.11943/j. issn.1006-9941.2017.05.001.
ZHENG Qi-long, LIU Hai-tao, HU Yi-wen, et al. Impact Damage and Dynamic Mechanical Behaviors of Azido Polyether Propellant at Low Temperature[J]. Chinese Journal of Energetic Materials, 2017, 25(5):354-359. DOI:10.11943/j. issn.1006-9941.2017.05.001.

复制
历史
  • 收稿日期: 2016-10-17
  • 最后修改日期: 2017-01-19
  • 录用日期: 2017-02-28
  • 在线发布日期: 2017-05-27
  • 出版日期: 2017-05-31