Mechanical Property of Paraffin/HTPB Fuel
Author:
Affiliation:

1.Science and Technology on Combustion, Internal Flow and Thermo-Structure Laboratory, Northwestern Polytechnical University, Xi′an 710072,China;2.Shanghai Space Propulsion Technology Research Institute, Shanghai 201109, China;3.Xi''an Aerospace Chemical Propulsion Co. Ltd., Xi′an 710025, China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
    摘要:

    为了研究端羟基聚丁二烯(HTPB)体系质量分数以及温度对石蜡/HTPB燃料力学性能的影响,制备了7种不同配方石蜡/HTPB拉伸试件,并使用万能材料试验机以10 mm·min-1拉伸速率进行了单轴拉伸实验,分析了燃料的最大抗拉强度、断裂伸长率和初始弹性模量变化规律。结果表明,随着HTPB体系质量分数增加,燃料的断裂伸长率增大,而最大抗拉强度和初始弹性模量皆减小;当环境温度较高(接近石蜡熔点58 ℃)时,燃料的最大抗拉强度和初始弹性模量皆随着HTPB质量分数增加而增大;燃料的最大抗拉强度随温度降低而逐渐增大,其中当温度由20 ℃降低至-40 ℃时,H20燃料最大抗拉强度由1.189 MPa升高至2.150 MPa;以HTPB体系为基体、石蜡为填料的石蜡/HTPB燃料,在其基体与填料的界面上存在相互阻滞作用力,可提高燃料的力学性能。

    Abstract:

    To study the effect of mass fraction of hydroxyl-terminated polybutadiene (HTPB) system and temperature on the mechanical properties of paraffin/HTPB fuels, seven kinds of paraffin/HTPB tensile specimens with different formulations were prepared, and the unidirectional tensile experiments were carried out by an universal materials testing machine at a tensile rate of 10 mm·min-1. The variation law of maximum tensile strength, elongation at break and the initial elasticity modulus of the fuel were analyzed. Results show that the fracture elongation of fuel increases with the increase of mass fraction of HTPB system, while the maximum tensile strength and the initial elasticity modulus decrease. When ambient temperature approachs the melting point of 58 ℃ for paraffin, the maximum tensile strength and initial elasticity modulus of the fuel increase with increasing the mass fraction of HTPB. The maximum tensile strength of fuel increases gradually with decreasing the temperature. In which, when the temperature decreases from 20 ℃ to -40 ℃, the maximum tensile strength of H20 fuel increases from 1.189 MPa to 2.150 MPa. The paraffin /HTPB fuel of HTPB system as matrix and paraffin as filler has mutual block acting force on the interface between its matrix and filler, which can increase the mechanical performance of the fuel.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

王印,王飞,胡松启,等.石蜡/HTPB燃料的力学性能[J].含能材料, 2019, 27(5):398-403. DOI:10.11943/CJEM2018153.
WANG Yin, WANG Fei, HU Song-qi, et al. Mechanical Property of Paraffin/HTPB Fuel[J]. Chinese Journal of Energetic Materials, 2019, 27(5):398-403. DOI:10.11943/CJEM2018153.

复制
历史
  • 收稿日期: 2018-06-08
  • 最后修改日期: 2019-01-09
  • 录用日期: 2018-09-13
  • 在线发布日期: 2018-12-19
  • 出版日期: 2019-05-25