Morphology Controlling Technique for Submicron CL-20
Author:
Affiliation:
Fund Project:
Article
|
Figures
|
Metrics
|
Reference
|
Related
|
Cited by
|
Materials
Abstract:
The submicron CL-20 was prepared by solvent-nonsolvent method with different surfactants, and the influence factors about various kinds, quality and injecting styles of surfactants were analyzed. Results show that the uniform and block-like CL-20 with 1 μm, 2 μm are obtained using 2 g raw materials CL-20 with 3.5 mL 2% polyvinyl alcohol (PV), and with 6.5 mL 5% polyoxyethylene ether (PT) respectively. The particle with 1 μm and elliptoid uniform and narrow particle-size distribution are obtained by watering pot injecting method with 6.5 mL 5% PT. CL-20 has higher heat sensitivity and is still ε polymorph after fine.
Reference
Related
Cited by
0
Article Metrics
PDF:
HTML:
Abstract:
Cited by:
Get Citation
杨利,王绍宗,赵鹏娟,等.超细CL-20晶形控制技术研究[J].含能材料,2008,16(3):254-257. YANG Li, WANG Shao-zong, ZHAO Peng-juan, et al. Morphology Controlling Technique for Submicron CL-20[J]. Chinese Journal of Energetic Materials,2008,16(3):254-257.