    Abstract:

    To quantitatively investigate the evolution of surface mesoscopic damagein nitrate ester plasticized polyether (NEPE) propellant during tension before and after aging, thermal accelerated aging tests were conducted with different aging days (0, 7 d, 40 d, 80 d). An in-situ tensile machine combined with field emission scanning electron microscopy (FE-SEM) was employed for in-situ tensile testing, after which the captured images underwent digital processing. The fractal dimension was applied to quantitatively characterize and analyze the evolution of mesoscopic damage in the propellant at different aging stages. The differences between porosity method and fractal dimension method in characterizing mesoscopic damage before and after aging were studied. Results indicate that fractal dimension successfully captures the apparent damage evolution of NEPE propellant over different aging stages. During tension, for elongation below 20%, the fractal dimension rises relatively quickly with elongation. In the 20%-60% elongation range, the fractal dimension still increase with elongation, though at a reduced rate. Moreover, longer aging times were found to enhance the linear correlation between fractal dimension and elongation in this stage. Beyond 60% elongation, the fractal dimension shows irregular variation with elongation for all aging stages. Differences emerged between the porosity method and the fractal dimension method when characterizing the tensile process, especially after aging. While the porosity method mainly measuresthe area fraction of pores, the fractal dimension method characterizes the roughness and complexity of the surface morphology.

    Reference
    Related
    Cited by
Article Metrics
  • PDF:
  • HTML:
  • Abstract:
  • Cited by:
Get Citation

张涛,姬永超,李卓,等.基于分形维数的老化NEPE推进剂拉伸损伤演化表征与分析[J].含能材料,2026,34(2):130-137.
ZHANG Tao, JI Yong-chao, LI Zhuo, et al. Characterization and Analysis of Tensile Damage Evolution in Aged NEPE Propellant Based on Fractal Dimension[J]. Chinese Journal of Energetic Materials,2026,34(2):130-137.

Cope
History
  • Received:July 11,2025
  • Revised:December 30,2025
  • Adopted:December 15,2025
  • Online: December 22,2025
  • Published: