Influence Factors of Slow Cook-off Characteristic for Solid Propellant
Author:
Affiliation:

Research Center of Solid Propellant Safety Technology of Aerospace Industry,Research Center of Solid Propellant Safety Technology of Aerospace Industry,Research Center of Solid Propellant Safety Technology of Aerospace Industry,Research Center of Solid Propellant Safety Technology of Aerospace Industry,Hubei Institute of Aerospace Chemotechnology,Hubei Institute of Aerospace Chemotechnology,Research Center of Solid Propellant Safety Technology of Aerospace Industry,Research Center of Solid Propellant Safety Technology of Aerospace Industry,Research Center of Solid Propellant Safety Technology of Aerospace Industry

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
    摘要:

    以HTPE推进剂、GAP推进剂为对象,采用慢速烤燃试验装置结合热电偶测温及传感器测压技术,研究了固体推进剂慢速烤燃特性的影响因素,包括配方组成、燃速、升温速率、约束条件、自由体积等。HTPE推进剂具有优异的慢速烤燃特性,10% HMX的加入使其慢速烤燃的响应程度增加,自由体积对其慢速烤燃的响应程度没有明显影响;燃速从10.1 mm·s-1增加到32.2 mm·s-1,升温速率从3.3 ℃·h-1增加到1 ℃·min-1,对GAP推进剂慢速烤燃的响应程度影响较小;增加夹板约束后,HTPE推进剂和GAP推进剂慢速烤燃的响应程度增加。

    Abstract:

    The influence factors of slow cook-off characteristic of solid propellant were studied with the object of HTPE propellant and GAP propellant by means of slow cook-off experimental device and thermocouple and pressure transducer, including composition, burning rate, heating rate, restriction condition, and free volume. HTPE propellant has a very excellent slow cook-off characteristic, hut the addition of HMX increases the response extent of slow cook-off, and free volume has not obvious effect on the response extent of slow cook-off. The burning rate from 10.1 mm·s-1 to 32.2 mm·s-1 and the heating rate from 3.3 ℃·h-1 to 1 ℃·min-1 have scarcely effect on the response extent of slow cook-off characteristic of GAP propellant. The response extent of slow cook-off becomes more violent after increasing restriction condition for HTPE propellant and GAP propellant.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

赵孝彬,李军,程立国,等.固体推进剂慢速烤燃特性的影响因素研究[J].含能材料, 2011, 19(6):669-672. DOI:10.3969/j. issn.1006-9941.2011.06.016.
ZHAO Xiao-bin,LI Jun, CHENG Li-guo, et al. Influence Factors of Slow Cook-off Characteristic for Solid Propellant[J]. Chinese Journal of Energetic Materials, 2011, 19(6):669-672. DOI:10.3969/j. issn.1006-9941.2011.06.016.

复制
历史
  • 收稿日期: 2011-09-27
  • 最后修改日期: 2011-11-07
  • 录用日期: 2011-11-08
  • 在线发布日期: 2012-02-22
  • 出版日期: